Stellite 31

Stellite 31 is a cobalt base superalloy (CoCrNiW) with high wear and corrosion resistance, excellent stress-rupture properties, resistance to thermal and mechanical shock and corrosion resistance. It is commonly used in the hottest sections of industrial gas turbines.